All raw material must be treated in natural cultivation for more steady in wood materal quality.
木材经过充裕的自然养生,使材质稳定。
Drying and degreasing
干燥脱脂
After drying and degreasing by five step in 48 hours, raw meaterial water contents are controled balance rate 8%--10%
通过48小时5个步骤的处理,有效将木材的含水量控制在8%-12% 平衡之内。
2,Superior perfect technique in process
卓越,完美的技术加工过程
Interlock
指接
Interlocking linking ends between Wood materials for promoting materail application and stability.
将方料纵长方向手指交错般连接,不仅提高木材的利用率,更增强木材的稳定性。
Intergrate spelling
集成拼板
After piled up in 48hour and heavy pressure in 2hours , then go into diging and flat plane.
指接堆放48小时,经过刨切后,再重压2小时,方可进入后面的冲料,刨切等工序。
Filling
填充
Using 4cm thickness filling plane,for preventing heavy hit and deformed.
我们用4cm后的指接板为填充料,大大提高木门的抗冲击度和抗变形能力。
Heavy pressure for single plane
压实木单板
Using 100ton pressurer pressed various plane in 2 minute below 98c.
使用100吨压机冷压2两分钟,压机温度不能超过98度。
Trimming
修边,砂光
products Trimed careful in handcraft are more perfected than machine.
手工能做到机器无法达到的完美效果。
Inspection
检验
Strict inspection through all process ensures the best quality to you.
严格的检验贯穿产品的整个生产过程。
木门以杉木为龙骨,采用合理的复合形式,确保木门久不变形和榫接 处永不开裂,木材蒸气烘干.精致加工.设计新潮.款设新颖. 本品按装适应性强,具有美观.平整.耐用.立体感强.隔音效果好,真 诚面向工薪用户和装璜按装单位.多种款设可供选择,卧室.厨房.办公室. 会议室.卫生间.阳台门.应有尽有.特殊式样和尺寸可加工定做. (长*宽*厚)单位(mm):门标准2050*800*40 2000*800*40 1950*700*40